Electrolytic Gold, Silver Refining
5K to 10K gold: Melt your 5K - 10K gold and cast an ingot. Place the gold ingot in the unit, fill the unit with electrolyte and turn on the power supply. 12-24 hours later, remove the anode section and wash the gold with water. Remove the disposable ashless paper bag with refined gold from the anode section. 10K and higher: