Activation of the carbothermic reduction of manganese ore
A sample of commercial manganese ore was obtained from a mine site in Western Australia and comprised lumps which were typically >30 mm. One lump was smashed using a hammer to <5 mm and then ground in a ball mill for 2 min; the resultant powder was screened at 212 μm and the oversize reground. This cycle was repeated …