Influence of physical and chemical parameters on ultrafine fluorspar …
The formation of slime particles in processes of minerals grinding limits froth flotation. Minera de Orgiva S.L. (Spain) produces slime sludge containing 41.05% of CaF 2 from a fluorite ore. Slimes have a very small particle diameter with very high specific surface area making this material difficult to process by froth flotation even when the grade of …