Superplasticity in tungsten-rhenium alloys
high elongations at 3630° F (2000° C) for tungsten alloys containing 20- to 30-atomic percent rhenium is reflected in the tensile strengths, which exhibit a distinct minimum in the vicinity of 28-atomic-percent rhenium (fig. 3). To determine the effects of annealing temperature on the tensile properties, speci mens were annealed at 3090° F ...