High-yield production of graphene flakes using a novel
3.1 Effect of the rotational speed of the rotational tool on graphene flakes. The graphite powder was intercalated in H 2 SO 4 electrolyte at the applied voltage of ± 1 V for 1 h under different rotational speeds of the rotational tool ranging from 0 to 2500 rpm in 500 rpm intervals. Then, the expanded graphite was exfoliated at the rotational speed of the …